The entire hook was cleaned and restored in 19 seconds.

The Challenge:  A painting contractor was hired to clean, repair, and recoat specialized hanger hooks coated with a thick and extremely hardened powder coat.  They were forced to bake and hand-scrape the hooks to remove the coating because abrasive blasting was not effective.  Even silicon carbide could barely dent the coating after minutes of blasting in a small area.

The 10X Breakthrough:  As seen in the photos, 10X abrasive immediately cut through the thick powder coating and left a clean, profiled surface ready for recoating.  The entire hook was cleaned and restored in 19 seconds.